Sign In | Join Free | My uabig.com
China Sun On Plastic Moulding Limited logo
Sun On Plastic Moulding Limited
Sun On Plastic Moulding Limited
Site Member

3 Years

Home > Injection Molding Solution >

OEM Silver Wire Plastic Injection Molding Solutions

Sun On Plastic Moulding Limited
Contact Now

OEM Silver Wire Plastic Injection Molding Solutions

MOQ : 100pcs

Price : Negotiable

Payment Terms : T/T

Supply Ability : More than 1 million

Delivery Time : 30day

Packaging Details : As the customer required

Place of Origin : CHINA

Brand Name : OEM

Certification : ISO

Emphasize : Analysis Of The Causes And Countermeasures Of Silver Stripes Or Material Flowers In Products

Contact Now

silver wire

  • Analysis Of The Causes And Countermeasures Of Silver Stripes Or Material Flowers In Products

Silver wire is also called silver grain or material flower, is in the product table and along the flow sentence appears similar to the phenomenon of silver hair white silk stripes. The main reason for the defects is the interference of gas (mainly water vapor, decomposition gas, solvent gas, air).

Cause Cuntermeasure
Forming condition

1. The injection molding speed is too fast

2. The temperature of the material is too high

4. The screw speed is too fast

5 melt when the back pressure is not appropriate, too much lead to shear, too low lead to bad exhaust

6.

The use of the injection feed machine has a long retention time

1. Reduce the speed or use graded glue

2. Reduce to the appropriate hardening temperature

3. Dry the material thoroughly

4. Set the appropriate speed

5. Set back pressure according to different conditions

6. Switch to the right model

Die

1. The runner and gate are too small, so that the shear is too large

2. Bad exhaust

3. There is no residual economy outside the cold material and gate, resulting in cold material

1. Increase the runner and gate

2. Increase and improve exhaust gas

3. Set S cold feed well. Improved gate

Product Design

1. Not enough R in the corner

2. Improper placement of gate and bar

3. Uneven wall thickness should be injected at high speed respectively

1. Set R Angle for smooth flow

2. Rearrange the gate

3. Improve product thickness

Material

1. More gas is produced when melting

2. Materials mixed with other miscellaneous materials

3. The recipe is too ripe to revive

1. Change to the material with less gas. 2. Carefully refueling

3. Reduce the proportion or use no raw materials

Other · The influence of release agent, Shan stain, etc avoid using


Product Tags:

Silver wire Injection Molding Solution

      

plastic Injection Molding Solutions

      

Silver wire plastic molding solutions

      
Wholesale OEM Silver Wire Plastic Injection Molding Solutions from china suppliers

OEM Silver Wire Plastic Injection Molding Solutions Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Sun On Plastic Moulding Limited
*Subject:
*Message:
Characters Remaining: (0/3000)